Community Training on Converting Wood Waste into Charcoal Using a Vertical Semi-Vacuum Kiln
DOI:
https://doi.org/10.68728/jrlk.v1i2.21Keywords:
Wood waste, Laban wood, Charcoal, Vertical semi-vacuum kiln, CarbonizationAbstract
Wood waste in Aceh is often left unused or burned openly, limiting its economic value and contributing to environmental pollution. This study aimed to design and evaluate a vertical semi-vacuum kiln to convert laban wood into charcoal as a potential community technology. The kiln featured a vertical carbonisation chamber and a system designed to restrict oxygen supply. We assessed performance using 20 kg of dried laban wood per trial. We recorded reactor temperature, initial biomass mass, final charcoal mass, charcoal yield, and observable physical characteristics across four 90-minute trials. The average final temperature reached 289°C, and each trial produced an average of 7.0 kg of charcoal, corresponding to a 35% yield. Individual yields ranged from 34% to 36%. The charcoal was generally dark, dry, relatively hard, and visually uniform, although one trial showed slightly incomplete carbonisation. A separate comparison reported yields of 40%, 35%, and 30% after 60, 90, and 120 minutes, respectively, at a stated temperature of 289°C; the 90-minute product received the best visual quality rating. The results suggest that longer processing reduced solid yield under the reported conditions, while the selected operating time balanced yield and visual quality. The kiln successfully produced charcoal from laban wood and may support local wood-waste utilisation. Direct pressure measurements, standardised charcoal analyses, and community implementation are needed to establish its broader performance and practical benefits.